How to Optimize Your Printing
Based on the properties of ABS-GF, it’s strongly recommended to consider the following tips to realize best performance:
1. Enclosure
An enclosed chamber helps maintain a consistent temperature around your print, reducing warping and improving print quality.
2. Use Brim
Adding a brim can significantly reduce warping by increasing the adhesion surface area.
3. Dry Your Filament
Although drying ABS-GF is optional, it's strongly recommended to dry it to prevent poor layer adhesion and brittleness.
Drying Condition:
Blast Drying Oven: 80 °C, 8h
X1 Series Heatbed: 90 - 100 °C, 13h
4. Other Settings
Build Plate & Bed Temperature: Smooth PEI Plate (90-100 °C); Textured PEI Plate (90-100 °C)
Printing Speed: < 180 mm/s
Nozzle Temperature: 240 - 280 ℃
Part Cooling Fan: 0 - 60%
Annealing: 80 - 90 ℃, 6 - 12 hours
| Item Type: |
3D Printing Filament |
|---|---|
| Model: |
ABS-GF |
| Color: |
Gray |
| Material: |
Acrylonitrile Butadiene Styrene – Glass Fiber Reinforced |
| Filament Diameter (mm): |
1.75 |
| Weight (kg): |
1 |
| Density (g/cm3): |
1.08 |
| Heat Distortion Temp. (°C) |
99 |
| Melt Flow Index (g/10min): |
7.56 ± 1.4 |
| Elongation at Break (%): |
6.3 ± 1.2 |
| Tensile Strength (MPa): |
36 ± 3 |
| Extruder Temperature (°C): |
240 to 270 |
| Heatbed Temperature (°C) |
80 to 100 |
| Melting Temp |
202 |
| Bending Strength |
68 ± 4 |